[PP-TANK-OS v26.9] uptime: 20y acid_resist=OK leak=0 hotline: 18615586932
pp-tank — bash — 80×24

$ ./init pp_tank --spec=hardcore

loading acid_resistance module ... OK

loading weld_engine v2 (butt+extrusion) ... OK

一家把酸洗槽做成硬核系统的工厂

参数即代码,工艺即算法:板厚经过核算、焊缝经过测试、交付附带日志。不整虚的,一切以输出为准。

        ______________________________________
       |  ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~  |
       |  HCl 18% | 65 C | LEVEL OK | NO LEAK |
       |______________________________________|
      /________________________________________\
         ||                              ||
      ===++==============================++===

$

$

ls -l /products/

total 6 · 全部可定制,点击行询价

$

cat /etc/tank.conf

# 标准槽型配置,非标工况请提交参数重新编译

# pp_tank standard profiles

tank.material全新料均聚 PP(炉号可溯)
tank.thickness_range8mm .. 30mm # 按液深核算
tank.max_temp95C
tank.acid.hcl<= 31%
tank.frame槽钢骨架整体包覆
weld.methodbutt_fusion + extrusion # 双工艺
weld.strength>= 0.9 * base_material
qa.hydro_test24h # 满水静置,零渗漏出厂
warranty1y + lifetime_support
$

make tank --progress

标准流程五步,每步产出可验证的交付物

calc_structure [100%] 输出:结构计算书 + 三视图
cut_sheets [100%] 输出:数控下料单
weld_assembly [100%] 输出:焊缝布置记录
hydro_test_24h [100%] 输出:满水试验记录表
ship_and_log [100%] 输出:竣工图 + 检验单
$

man pp-tank | grep FAQ

能耐多高浓度的酸?

均聚 PP 长期耐受 31% 盐酸 / 50% 硫酸与大部分碱液;硝酸铬酸等强氧化性介质会建议改用 PVDF 方案,不硬接单。

交期多久?

常规槽型 7 天,非标 15 天,写进合同;拖一天按合同赔,这个 flag 立了十年没倒。

怎么证明不漏?

出厂前满水静置 24 小时,逐条焊缝检视并拍照,记录表随货同行——log 不说谎。

$

tail -f /var/log/news.log

$ contact --now

发送工况参数(介质 / 温度 / 尺寸),stdout 返回图纸与报价。

18615586932 [ EXECUTE ]